Irradiation-assisted stress corrosion cracking

  • Nuclear Reactor Baffle Bolt Problems Are Widespread Concern

    Public Service Enterprise Group (PSEG) anticipates extending Salem Nuclear Generating Station’s Unit 1 refueling outage, which began on April 14, so it can inspect, repair, and replace damaged baffle bolts within the plant’s reactor vessel, according to information presented in the company’s first quarter earnings announcement. A PSEG spokesperson told POWER that visual inspections at […]